MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin 1000P200 Polyetherimide (PEI)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: ULTEM 1000P200 Resin is an unreinforced amorphous polyetherimide (PEI) powder. This powder is available with an average particle size (D50) of 200 micron and a maximum particle size (D100) of 450 micron.. It may offer a high glass transition temperature (Tg) of 217°C. Features are excellent mechanical, electrical and dimensional properties up to high temperatures. The material may offer very good chemical resistance for an amorphous material and is inherently flame retardant. The material is RoHS Compliant. The base material is transparent amber colored.

Features: Hydrolytic Stability,Chemical Resistance,Miscible with epoxy,High Heat Resistance,Good dimensional stability,Flame Retardant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
Density 1.27 g/ccISO 1183
Water Absorption 0.25 %
@Time 86400 sec
ASTM D570
 0.25 %
@Time 86400 sec
ISO 62-1
Moisture Absorption 0.200 %23°C/50% RH/24 hrs; ISO 62-4
Moisture Absorption at Equilibrium 0.70 %23°C/50% RH; ISO 62-4
Water Absorption at Saturation 1.25 %ASTM D570
 1.25 %ISO 62-1
Viscosity 13 cP
@Load 5.00 kg,
Temperature 360 °C
MVR cc/10 min; ISO 1133
Melt Flow 9.0 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 106ISO 2039-2
 109ASTM D785
Ball Indentation Hardness 140 MPaH358/30; ISO 2039-1
Tensile Strength, Yield 110 MPa5 mm/min; ASTM D638
 110 MPa50 mm/min; ISO 527
 115 MPa50 mm/min; ASTM D638
Elongation at Break 50 %50 mm/min; ISO 527
 60 %5 mm/min; ASTM D638
 60 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ISO 527
 7.0 %5 mm/min; ASTM D638
 7.0 %50 mm/min; ASTM D638
Tensile Modulus 3200 MPa1 mm/min; ISO 527
 3350 MPa5 mm/min; ASTM D638
Flexural Strength 160 MPayld, 2.6 mm/min, 100 mm span; ASTM D790
 160 MPayield, 2 mm/min; ISO 178
 165 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3200 MPa1.3 mm/min, 50 mm span; ASTM D790
 3300 MPa2 mm/min; ISO 178
 3400 MPa2.6 mm/min, 100 mm span; ASTM D790
Poissons Ratio 0.36ASTM E132
Izod Impact Notched 53.0 JASTM D256
 50.0 J
@Temperature -30.0 °C
ASTM D256
 1335 J
@Thickness 3.20 mm
reverse notched; ASTM D256
Izod Impact, Unnotched 1800 J/mASTM D4812
 1540 J/m
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact, Notched 4.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 4.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Gardner Impact 36.0 JASTM D3029
Taber Abrasion, mg/1000 Cycles 10CS-17, 1 kg; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
 1.00e+17 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.9
@Frequency 1e+6 Hz
IEC 60250
 2.9
@Frequency 50.0 - 60.0 Hz
IEC 60250
 3.01
@Frequency 1.10e+9 Hz
 3.02
@Frequency 5.00e+9 Hz
 3.02
@Frequency 1e+10 Hz
 3.15
@Frequency 1000 Hz
ASTM D150
 3.15
@Frequency 100 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 19.7 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
 25.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 28.0 kV/mm
@Thickness 1.60 mm
in oil; ASTM D149
 32.7 kV/mm
@Thickness 1.60 mm
in air; ASTM D149
 33.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Dissipation Factor 0.00050
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0012
@Frequency 1000 Hz
ASTM D150
 0.0012
@Frequency 1.10e+9 Hz
 0.0015
@Frequency 100 Hz
ASTM D150
 0.0024
@Frequency 5.00e+9 Hz
 0.0027
@Frequency 1e+10 Hz
 0.0060
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 100 VIEC 60112
 150 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 52.0 µm/m-°C
@Temperature -20.0 - 150 °C
ISO 11359-2
 56.0 µm/m-°C
@Temperature -20.0 - 150 °C
ASTM E831
CTE, linear, Transverse to Flow 52.0 µm/m-°C
@Temperature -20.0 - 150 °C
ISO 11359-2
 54.0 µm/m-°C
@Temperature -20.0 - 150 °C
ASTM E831
Thermal Conductivity 0.220 W/m-KASTM C177
 0.220 W/m-KISO 8302
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 209 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 207 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 210 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 192 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 190 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 201 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 211 °CRate B/50; ASTM D1525
 211 °CRate B/50; ISO 306
 212 °CRate B/120; ISO 306
 215 °CRate A/50; ISO 306
Oxygen Index 47 %ASTM D2863
 47 %ISO 4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82570 / 290517

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.