MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Europrene® SOL R 72614 Styrene - Butadiene Copolymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Europrene® SOL R 72614 is a solution polymerized, oil extended styrene-butadiene random copolymer. The polymer is extended with a TDAE oil and contains a non-staining antioxidant. It is produced by batch polymerization process.

Key Features: Europrene® SOL R 72614 has a microstructure and molecular weight distribution designed to show a good trade-off between processability and final properties.

Main Applications: Silica-based compounds for low rolling resistance tire treads.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.75 %<= 0.75 %ASTM D5668
Mooney Viscosity 55
@Temperature 100 °C
55
@Temperature 212 °F
ASTM D1646
Vinyl Acetate Content 65 %65 %Referred to butadiene portion; Internal Method
Ash <= 0.20 %<= 0.20 %ASTM D5667
 
Chemical PropertiesMetricEnglishComments
Styrene Content 25 %25 %Bound; ASTM D5775
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -30.0 °C-22.0 °FInternal Method
 
Descriptive Properties
Oil Content (phr)37.5ASTM D5774

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENG192 / 124586

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.