MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Trigonox 141 Thermoset 2,5-Dimethyl-2,5-di(2-ethylhexanoylperoxy) hexane
Categories: Other Engineering Material

Material Notes: Trigonox 141 is a bi-functional perester used for curing unsaturated polyester and vinylester resins at high temperatures.

CAS number: 13052-09-0

EINECS/ELINCS No: 235-935-5

Applications: Thermoset: Trigonox 141, 2,5-Dimethyl-2,5-di(2-ethylhexanoylperoxy)hexane, is a di-functional perester which is used for the curing of unsaturated polyester resins at high temperatures. Trigonox 141 is preferred for the curing of UP resin based Hot Press Molding formulations (such as DMC and BMC) in the temperature range of 120 - 160°C. Trigonox 141 is preferably used in combination with a low reactive peroxide like Trigonox C or Trigonox BPIC-C75 and an optimal low Profile SMC formulation for the production of HPM parts with a Class A surface at short molding times. Polymerization of styrene: In suspension polymerization processes, Trigonox 141 can be used for the polymerization of styrene at approximately 90°C. Trigonox 141 has an activity comparable with Dibenzoyl peroxide (Perkadox L-W75). However, the bifunctional Trigonox 141 gives higher molecular weights of the polymer. Applying the same molecular weights means a reduction of polymerization time. Polymerization of acrylates and methacrylates: Trigonox 141 can be used as initiator for the solution (co)polymerization of acrylates and methacrylates in the temperature range of 80-160°C, amongst others for the manufacture of coatings. Trigonox 141 can also be applied as an initiator for the bulk and suspension (co)polymerization of acrylates and methacrylates

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.956 g/cc0.0345 lb/in³
Viscosity 80 cP80 cP
Storage Temperature <= 15.0 °C<= 59.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 35.0 °C95.0 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay0.92
Color= 20 Pt-Co
Content= 100 mg/kgInorganic + organic hydrolysable chloride
 = 2.2 %2,5-dihydroperoxy-2,5-dimethylhexane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1013 / 286536

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.