MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Huber Hymod® M932 SP Aluminum Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Huber Engineered Materials’ Hymod® M932 SP is a high surface area vinyl silane treated ATH product with a very precise, ultrafine particle size distribution specifically designed for low viscosity, high loading, and excellent processing characteristics. This product provides functional reinforcement, flame retardancy and smoke suppression in a variety of applications, such as acrylic, EPDM, EVA, SBR, polyester and polyolefin compounds.

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.42 g/cc2.42 g/cc
Bulk Density 0.350 g/cc0.0126 lb/in³Loose
 0.760 g/cc0.0275 lb/in³Packed
Particle Size 2.0 µm2.0 µmMedian Particle Diameter
Particle Mesh Size 325 Mesh325 Mesh99.99% through
Specific Surface Area 12 m²/g12 m²/g
 
Component Elements PropertiesMetricEnglishComments
Fe2O3 0.0070 %0.0070 %
Loss on Ignition(%) 34.6 %
@Temperature 550 °C
34.6 %
@Temperature 1020 °F
Na2O 0.12 %0.12 %soluble
 0.30 %0.30 %total
SiO2 0.0050 %0.0050 %
 
Descriptive Properties
Al(OH)3 (%)99.6
FunctionalityLow Viscosity Aid
 Smoke Suppression
Market/Application: ThermosetsRubber & Plastics

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EHUBER711 / 300817

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.