Celanese FORTRON ICE 506L PPS, 40% Glass Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polyphenylene Sulfide (PPS)
;
Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
Material Notes:
Fortron ICE 506L is a faster crystallizing version of Fortron 1140L6. It offers essentially the same characteristics of 1140L6 with improved crystallization efficiency for faster cycle times in complex geometries.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.60
g/cc
1.60
g/cc
ASTM D792
Density
1.65
g/cc
0.0596
lb/in³
ISO 1183
Water Absorption
0.020 %
@Temperature 22.8 °C
0.020 %
@Temperature 73.0 °F
24hr immersion; ASTM D570
Water Absorption at Saturation
0.020 %
0.020 %
ISO 62
Linear Mold Shrinkage, Flow
0.0020
-
0.0030
cm/cm
0.0020
-
0.0030
in/in
ASTM D955
0.0020
-
0.0060
cm/cm
0.0020
-
0.0060
in/in
ISO 294-4
Linear Mold Shrinkage, Transverse
0.0040
-
0.0060
cm/cm
0.0040
-
0.0060
in/in
ISO 294-4
0.0050
-
0.0070
cm/cm
0.0050
-
0.0070
in/in
ASTM D955
Melt Flow
19
g/10 min
19
g/10 min
ASTM D1238
Spiral Flow
21.5
cm
8.46
in
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
100
100
ISO 2039-2
100
100
ASTM D785
Tensile Strength at Break
195
MPa
28300
psi
5mm/min; ISO 527-2/1A
200
MPa
29000
psi
ASTM D638
Elongation at Break
1.9 %
1.9 %
5mm/min; ISO 527-2/1A
2.0 %
2.0 %
ASTM D638
Tensile Modulus
14.7
GPa
2130
ksi
50mm/min; ISO 527-2/1A
Flexural Strength
276
MPa
40000
psi
ASTM D790
285
MPa
41300
psi
ISO 178
Flexural Modulus
13.8
GPa
2000
ksi
ASTM D790
14.5
GPa
2100
ksi
ISO 178
Izod Impact, Notched
1.01
J/cm
1.90
ft-lb/in
ASTM D256
Izod Impact, Unnotched
5.87
J/cm
11.0
ft-lb/in
ASTM D256
Izod Impact, Notched (ISO)
10.0
kJ/m²
@Temperature -30.0 °C
4.76
ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
34.0
kJ/m²
@Temperature 23.0 °C
16.2
ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched
5.30
J/cm²
25.2
ft-lb/in²
ISO 179/1eU
5.30
J/cm²
@Temperature -30.0 °C
25.2
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched
1.00
J/cm²
4.76
ft-lb/in²
ISO 179/1eA
1.00
J/cm²
@Temperature -30.0 °C
4.76
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
>=
1.00e+15
ohm-cm
>=
1.00e+15
ohm-cm
IEC 60093
1.00e+16
ohm-cm
1.00e+16
ohm-cm
ASTM D257
Surface Resistance
>=
1.00e+15
ohm
>=
1.00e+15
ohm
IEC 60093
Dielectric Constant
3.5
@Frequency 1000 Hz
3.5
@Frequency 1000 Hz
ASTM D150
3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
ASTM D150
4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength
15.4
kV/mm
390
kV/in
short term; ASTM D149
28.0
kV/mm
711
kV/in
IEC 60243-1
Dissipation Factor
0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
ASTM D150
0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
ASTM D150
0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance
134
sec
134
sec
ASTM D495
Comparative Tracking Index
125
V
125
V
IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
26.0
µm/m-°C
14.4
µin/in-°F
ISO 11359-2
CTE, linear, Transverse to Flow
42.0
µm/m-°C
23.3
µin/in-°F
ISO 11359-2
Specific Heat Capacity
1.50
J/g-°C
0.359
BTU/lb-°F
Melting Point
280
°C
536
°F
10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi)
280
°C
536
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
265
°C
509
°F
ASTM D648
270
°C
518
°F
ISO 75-1, -2
Deflection Temperature at 8.0 MPa
215
°C
419
°F
ISO 75-1, -2
Glass Transition Temp, Tg
90.0
°C
194
°F
ISO 11357-1,-2,-3
Processing Properties
Metric
English
Comments
Processing Temperature
90.0
-
160
°C
194
-
320
°F
cavity
330
-
340
°C
626
-
644
°F
hot runner
Feed Temperature
60.0
-
80.0
°C
140
-
176
°F
Zone 1
290
-
300
°C
554
-
572
°F
Zone 2
310
-
320
°C
590
-
608
°F
Zone 3
330
-
340
°C
626
-
644
°F
Zone 4
330
-
340
°C
626
-
644
°F
Die Temperature
310
-
330
°C
590
-
626
°F
Melt Temperature
310
-
340
°C
590
-
644
°F
ISO 294
330
-
340
°C
626
-
644
°F
Mold Temperature
135
-
160
°C
275
-
320
°F
ISO 294
Drying Temperature
130
-
140
°C
266
-
284
°F
Dry Time
3.00
-
4.00
hour
3.00
-
4.00
hour
Moisture Content
<= 0.020 %
<= 0.020 %
Injection Pressure
50.0
-
100
MPa
7250
-
14500
psi
Hold Pressure
30.0
-
70.0
MPa
4350
-
10200
psi
Back Pressure
<=
3.00
MPa
<=
435
psi
Screw Speed
50
rpm
@Diameter 55.0 mm
50
rpm
@Diameter 2.17 in
75
rpm
@Diameter 40.0 mm
75
rpm
@Diameter 1.57 in
120
rpm
@Diameter 25.0 mm
120
rpm
@Diameter 0.984 in
Descriptive Properties
Injection molding
Yes
Injection speed
fast
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese FORTRON 1140L6 PPS, 40% Glass Reinforced
Celanese FORTRON ICE 504L PPS, 40% Specialty
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced
Celanese FORTRON 1140L0 PPS, 40% Glass Reinforced
Celanese FORTRON ICE 714A PPS, 65% Mineral / Glass Reinforced
PHCQ293 / 178748
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.