MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Colorite Polymers Elastichem 3511TX-02 Vinyl Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, complete traceability and lot identification of all components are maintained at Colorite.

  • Low coefficient of friction
  • Low gels
  • Improved physical properties
  • Non-sticking, even at 40 shore A
  • Self-frosting for extrusion
  • Self-frosting for injection molding
  • Excellent resiliency for product requiring peristaltic motion
  • Improved extrusion rates for low durometer compounds (i.e. 40-50A)

Information provided by Colorite Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35ASTM D2240
Tensile Strength, Ultimate 1112 psiASTM D638
Elongation at Break 525 %ASTM D638
Modulus of Elasticity 0.237 ksiASTM D638
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -57.5 °CTf; ASTM D746
Brittleness Temperature -63.0 °CXTb; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Colorite Polymers Elastichem 8011TX-02 Vinyl Compound
Colorite Polymers Elastichem 4011TX-02 Vinyl Compound
Colorite Polymers Elastichem 7011TX-02 Vinyl Compound
Colorite Polymers Elastichem 5011TX-02 Vinyl Compound
Colorite Polymers Elastichem 6011TX-02 Vinyl Compound

PCOL089 / 28808

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.