MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® B 38 FKA 000000 Nylon 6 (PA6), Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: PA 6 film-grade, medium to higher viscosity, with processing aid and slip agent, nucleated, in compliance with FDA for food contact

Application Examples: flat and blown film, flat film coextrusion for PA/PE composite films

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Moisture Absorption at Equilibrium 3.0 %3.0 %50% RH; ISO 62
Water Absorption at Saturation 10 %10 %ISO 62
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 235 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 455 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 40.0 MPa5800 psiISO 2093-1
Tensile Strength, Yield 35.0 MPa5080 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %>= 50 %50 mm/min, Nominal; ISO 527-1,-2
Elongation at Yield 25 %25 %50 mm/min; ISO 527-1,-2
Tensile Modulus 0.800 GPa116 ksi1 mm/min; ISO 527-1,-2
Flexural Yield Strength 20.0 MPa
@Strain 3.5 %
2900 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 0.700 GPa102 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 8.0 %8.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  7.50 kJ/m²
@Temperature -30.0 °C
3.57 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 50.0 kJ/m²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179-1eU
Charpy Impact, Notched  <= 0.500 J/cm²
@Temperature -30.0 °C
<= 2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
 18
@Frequency 100 Hz
18
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
@Thickness 1.00 mm
889 kV/in
@Thickness 0.0394 in
IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °F10°C/min (Dry); ISO 11357-1,-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °Finjection molding
Mold Temperature 40.0 °C104 °Finjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANW9275 / 208078

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.