MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crystex Composites Mykroy/Mycalex MM 371 Molding Grade Glass-bonded Mica Composite  (discontinued **)
Categories: Ceramic; Glass; Glass Ceramic

Material Notes: Discontinued. Replaced with RoHS compliant grade MM451.

Natural mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt). This leaded grade is not ROHS compliant.

This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwide. Glass-Bonded Mica is the only inorganic material to bridge the performance materials gap between organic plastics and ceramics.

This unique high performance technical ceramic is a union of finely powered electrical quality glass and precisely defined and classified mica. The union of mica and glass takes place under simultaneous pressure and heat, transforming the materials into a new composition that inherits all the insulating advantages of both constituents.

These materials are easily machined, mold like plastic, and have a wide range of operating temperatures. They find applications in the aircraft, laser, communications, aerospace, cryogenic, electronic, radiation, semiconductor, computer, automotive, and power distribution industries.

Typical data below provided by Mykroy/Mycalex Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.80 g/cc0.173 lb/in³
Moisture Absorption at Equilibrium 0.00 %0.00 %Nil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A 4747
Hardness, Rockwell H 9090
Tensile Strength, Ultimate 44.8 MPa6500 psi
Flexural Strength 68.9 MPa10000 psi
Compressive Strength 241 MPa35000 psi
Izod Impact, Notched 4.27 J/cm8.00 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cm
Surface Resistivity per Square 1.00e+15 ohm1.00e+15 ohm
Dielectric Constant 12.5
@Frequency 1e+6 Hz
12.5
@Frequency 1e+6 Hz
Dielectric Strength 13.8 kV/mm350 kV/in
Dissipation Factor 0.0060
@Frequency 1e+6 Hz
0.0060
@Frequency 1e+6 Hz
Dielectric Loss Index 0.075
@Frequency 1e+6 Hz
0.075
@Frequency 1e+6 Hz
Arc Resistance 300 sec300 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.2 µm/m-°C
@Temperature 350 °C
6.22 µin/in-°F
@Temperature 662 °F
 13.02 µm/m-°C
@Temperature 25.0 °C
7.233 µin/in-°F
@Temperature 77.0 °F
Specific Heat Capacity 1.046 J/g-°C0.2500 BTU/lb-°F
Thermal Conductivity 0.930 W/m-K6.45 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 370 °C698 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AR-Glass Fiber, Generic
Thermal Transfer Composites PRIMEX ULTRA™ MCT-487™ Aluminum Silicon Carbide Composite, Reinforced
Crystex Composites Mykroy/Mycalex 555 Molding Grade Glass-bonded Mica Composite
Crystex Composites Mykroy/Mycalex MM 411 Moldable Glass-Mica Composite
Crystex Composites Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite

CMYKROY28 / 1660

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.