MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polytek PT Flex 85 Fast-Curing, Pourable Polyurethane Casting Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: PT Flex Liquid Rubbers are flexible, fast-curing rubbers, for use in prototyping and model making applications. They are excellent for casting decorative objects, production parts, tools, models, patterns, duplicate masters and more. With the addition of PolyColor Dyes, PT Flex products can be used to cast parts of any color.

Product Line Features:

  • Easy 1A:1B mix formulations
  • Low viscosity
  • Reproduces fine detail
  • Low shrinkage on cure
  • Rapid demold time
  • Castable in large masses

Information provided by Polytek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/cc
Viscosity 750 cPMixed
Linear Mold Shrinkage 0.0016 in/inUpon Cure
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85
Tensile Strength 1064 psi
Elongation at Break 250 %
Modulus of Elasticity 2.70 ksi
Tear Strength 190 pliDie C Tear
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hourDemold Time
 5.00 minPour Time
 
Descriptive Properties
Cured ColorAmber
Mix Ratio By Weight1A:1B
Specific Volume26.2 in3/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPTK5051 / 251043

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.