MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt POLYCOR® 24 X Series Gel Coat
Categories: Polymer; Thermoset

Material Notes: The 24X series gelcoats are enamel like coatings developed for the composites and fiberglass industry. These gelcoats are used as an enamel coating, similar to paint and are often used to hide any fiberglass pattern inside the part. This series is suitable for water immersion and can be used if high blister resistance is not a major concern. The 24X series gelcoat can also be used to protect the laminate against U.V. rays. 24X series gelcoat is more like a polyester paint and offers improved cosmetic surface of fiberglass. 24X series gel coats are sag resistant and have a fast curing system.
  • Formulated for spray and roll application.
  • Fast gel time and cure time that provide a good cure.
  • Require only the addition of a proper amount of MEKP to cure.
  • Easy to spray and roll
  • Good hiding abilities.
These gelcoats are available in a wide range of appealing colors. Color matching is available on request. The numbers following: 24X…indicate the product color code. For parts in contact with water, (severe conditions) an NPG/ISO base gelcoat is recommended. For fire retardant properties, a specific fire retardant base gelcoat is recommended. Parts that have to be assembled should be sanded before, to obtain a good adherence. 24 series gelcoat may be applied by brush, roller or spray.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 3400 - 5500 cP3400 - 5500 cPRVF #4 Spindle @ 20 rpm
 
Processing PropertiesMetricEnglishComments
Cure Time 45.0 - 60.0 min
@Temperature 25.0 °C
0.750 - 1.00 hour
@Temperature 77.0 °F
tested @ 1,8% Norox MEKP 925 à 25°C
Gel Time 6.00 - 12.0 min6.00 - 12.0 mintested @ 1,8% Norox MEKP 925 à 25°C
 
Descriptive Properties
Sag ResistanceGood at 20 mils
Thixotropic Index<6.52/20 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon 51112R013 0.013" (0.330 mm) Cured, Self Fusing, Silicone Rubber with Fiberglass Substrate
Rogers Arlon 440-638RF 0.0055" (0.140 mm) Style 1165 Plain Weave, Prime Coated Fiberglass
Solvay 200TFNP PTFE-coated fiberglass cloth
Saint-Gobain COHRlastic® 300AR Reinforced Silicone Sponge/Aggressive Acrylic Adhesive Pressure Sensitive Tape
Saint-Gobain Chemfab® TCN® 2000 High-Strength Leno Weave Nomex/Fiberglass Belting Material

PPOLYN9262 / 231857

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.