MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) RHODOLINE® 990 Surfactant
Categories: Fluid

Material Notes: Standard Applications: RHODOLINE® 990 is an APE-free, silicone-free and oil-free defoamer for waterbased systems. It is widely used in paints, inks and adhesives. RHODOLINE® 990 has little impact on the gloss and can be used in clear and gloss coatings. RHODOLINE® 990 is recommended for use at concentration of 0.2 to 0.4%. It may be used as received or predispersed in water.

Chemical Name: Defoamer

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 - 1.03 g/ccRP-17617
pH 5.0 - 8.05% solution; RP-0420
Viscosity 500 - 1000 cPRP-0596
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceAmber, slightly opaque liquidRP-0064

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay RHODOLINE® DF-665 Surfactant
Syensqo (Solvay Specialty Polymers) RHODOLINE® 999 Surfactant
Solvay RHODOLINE® DF-988 Surfactant

PSOLVAY808 / 218536

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.