MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe Graph-Mo® Cold Work Tool Steel (ASTM O6)
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel; Tool Steel; Cold Work Steel; Oil-Hardening Steel

Material Notes: Graph-Mo tool steel is an oil-hardening, graphitic tool steel with outstanding resistance to metal-to-metal sliding wear and galling. The steel contains a uniform dispersion of graphite particles which impart excellent machinability and non-seizing characteristics. The graphite particles make the steel self-lubricating in dry environments, and help to retain oil in lubricated environments. Graph-Mo tool steel can be hardened to over 60 Rockwell C from a relatively low hardening temperature, which minimizes size change and distortion during heat treatment. Typical applications include thread gauges, master gages, cams, bushings, sleeves, meat granulator plates, arbors, forming rolls, shear blades, punches, dies, bar feed guides and other machine tool parts.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.70 g/cc
Density 0.278 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 62Air Cooled from 774°C, 30 minutes
 64Air Cooled from 871°C, 30 minutes
 65.5Air Cooled from 802°C, 30 minutes
Modulus of Elasticity 30000 ksi
Machinability 130 %1% Carbon Steel
Izod Impact Unnotched 20.0 ft-lbOil Quenched from 788°C; 250°C Temper Temperature
 95.0 ft-lbOil Quenched from 788°C; 538°C Temper Temperature
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.15 µm/m-°C
@Temperature 21.0 - 204 °C
 12.94 µm/m-°C
@Temperature 21.0 - 538 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.45 %
Iron, Fe 96.4 %
Manganese, Mn 1.0 %
Molybdenum, Mo 0.25 %
Silicon, Si 0.90 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carpenter O6 Graphitic Tool Steel (AISI O6)
AISI Type O6 Tool Steel
Crucible Steel HALGRAPH® Tool Steel, AISI O6
ATI Allegheny Ludlum 06 Tool Steel, UNS T31506
AISI Type O1 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 425°C

NTIMK116 / 19463

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.