MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Glass Fiber Reinforced

Material Notes: Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:
  • Highest mechanical properties at high temperatures
  • Excellent resistance to wear and low friction
  • Outstanding flow for easy processing and exceptional design freedom
  • Stanyl High Flowgrades that match the best flowing LCPs while maintaining a high level of mechanical properties

Key Applications:

  • Automotive: Powertrain components, Charge-air coolers, EPS and ETC gears, Motor Sensors, Auto connectors, Chain tensioners
  • E&E: Connectors, Microswitches, Bobbins, Memory modules, Motor components, Industrial, Specialty films and fibers, Consumer appliances

    Information provided by DSM.

    Former DSM Engineering Plastics product line is now with Envalior.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 1.41 g/cc(DAM); ISO 1183
    Water Absorption 9.5 %DAM; Sim. to ISO 62
    Moisture Absorption at Equilibrium 2.6 %Humidity Absorption (DAM); Sim. to ISO 62
    Linear Mold Shrinkage, Flow 0.0050 cm/cmDAM; ISO 294-4
     0.013 cm/cmDAM; ISO 294-4
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength at Break 115 MPaISO 527-1/-2
    Elongation at Break 7.0 %ISO 527-1/-2
    Tensile Modulus 6.00 GPaISO 527-1/-2
    Charpy Impact Unnotched 7.00 J/cm²
    @Temperature -30.0 °C
    ISO 179/1eU
     9.00 J/cm²
    @Temperature 23.0 °C
    ISO 179/1eU
    Charpy Impact, Notched 1.00 J/cm²
    @Temperature -30.0 °C
    ISO 179/1eA
     1.90 J/cm²
    @Temperature 23.0 °C
    ISO 179/1eA
    Tensile Creep Modulus, 1000 hours 4500 MPaISO 899-1
     
    Electrical PropertiesOriginal ValueComments
    Volume Resistivity 1.00e+9 ohm-cmIEC 60093
    Surface Resistance 1.00e+13 ohmIEC 60093
    Dielectric Constant 4.7
    @Frequency 1e+6 Hz
    IEC 60250
     16
    @Frequency 100 Hz
    IEC 60250
    Dielectric Strength 20.0 kV/mmIEC 60243-1
    Dissipation Factor 0.010
    @Frequency 1e+6 Hz
    IEC 60250
     0.060
    @Frequency 100 Hz
    IEC 60250
    Comparative Tracking Index 300 VIEC 60112
     
    Thermal PropertiesOriginal ValueComments
    Melting Point 295 °C10°C/min (DAM); ISO 11357-1/-3
     
    Descriptive Properties
    Heat Stabilized or Stable to HeatYes
    Injection MoldingYes
    PlatableYes
    With FillersYes

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Envalior Stanyl® TW200F6 PA46-GF30, Dry, 30% Glass Filled, Heat Stabilized
    Envalior Stanyl® TW200F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America)
    Envalior Stanyl® TW200F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America)
    Avient Lubri-Tech™ NN-30CF/15T FR Nylon 6/6 - 30% Carbon Fiber - 15% PTFE
    Envalior Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)

    PDSMEU492 / 31367

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.