Properties and applications: SIPERNAT represents a specific product range of precipitated silica, aluminum and calcium silicates. SIPERNAT D 17 is a hydrophobic silica and not wettable by water. Its primary application is as anti-caking agent.- fire extinguishing powders (anticaking)
- manufacture of defoamers/antifoams (fast foam destruction)
- chemicals (flowability, anticaking)
- HTV/RTV-2C/LSR silicone rubber (reinforcing filler)Information provided by Evonik
|