System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
SABIC LNP™ THERMOCOMP™ Compound PF008S Polyamide 6 (Nylon 6) (Asia)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
Material Notes:
LNP THERMOCOMP PF008S compound is based on Nylon 6 resin containing 40% glass fiber. Added features of this grade include: Heat Stabilized.
Features: High Stiffness,Heat Stabilized,Structural
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.47
g/cc
0.0531
lb/in³
ASTM D792
1.47
g/cc
0.0531
lb/in³
ISO 1183
Moisture Absorption
0.150 - 0.250 %
0.150 - 0.250 %
Injection Molding
0.980 %
0.980 %
23°C/50% RH/24 hrs; ASTM D570
1.26 %
1.26 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.0020
-
0.0040
cm/cm
0.0020
-
0.0040
in/in
24hrs; ASTM D955
0.0020
-
0.0040
cm/cm
0.0020
-
0.0040
in/in
24hrs; ISO 294
Linear Mold Shrinkage, Transverse
0.0060
-
0.0080
cm/cm
0.0060
-
0.0080
in/in
24hrs; ASTM D955
0.0060
-
0.0080
cm/cm
0.0060
-
0.0080
in/in
24hrs; ISO 294
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
183
MPa
26500
psi
ASTM D638
186
MPa
27000
psi
ISO 527
Elongation at Break
3.3 %
3.3 %
ASTM D638
3.3 %
3.3 %
ISO 527
Tensile Modulus
12.67
GPa
1838
ksi
50 mm/min; ASTM D638
12.99
GPa
1884
ksi
1 mm/min; ISO 527
Flexural Strength
278
MPa
40300
psi
ASTM D790
278
MPa
40300
psi
ISO 178
Flexural Modulus
9.25
GPa
1340
ksi
ASTM D790
9.53
GPa
1380
ksi
ISO 178
Izod Impact Notched
133
J
98.1
ft-lb
ASTM D256
Izod Impact, Notched (ISO)
17.0
kJ/m²
8.09
ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
92.0
kJ/m²
43.8
ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy
25.0
J
18.4
ft-lb
peak; ASTM D3763
Impact Test
21.0
J
15.5
ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
208
°C
406
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
195
°C
@Thickness 3.20 mm
383
°F
@Thickness 0.126 in
unannealed; ASTM D648
Processing Properties
Metric
English
Comments
Zone 2
265
-
275
°C
509
-
527
°F
Zone 3
275
-
290
°C
527
-
554
°F
Melt Temperature
265
-
275
°C
509
-
527
°F
Injection Molding
Mold Temperature
80.0
-
95.0
°C
176
-
203
°F
Drying Temperature
80.0
°C
176
°F
Injection Molding
Dry Time
4.00
hour
4.00
hour
Injection Molding
Back Pressure
0.300
-
0.700
MPa
43.5
-
102
psi
Screw Speed
30
-
60
rpm
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH81785 / 289732
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.