MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastics Tepcon M450 Acetal-copolymer (POM), Super High Fluidity, High Cycle
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Information provided by PolyPlastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 63.0 MPa9140 psiISO 527-1, 2
Elongation at Break 27 %27 %ISO 527-1, 2
Tensile Modulus 2.80 GPa406 ksiISO 527-1, 2
Flexural Strength 89.0 MPa12900 psiISO 178
Flexural Modulus 2.55 GPa370 ksiISO 178
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
Dielectric Strength 19.0 kV/mm483 kV/inIEC 60243-1
Comparative Tracking Index >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C
@Temperature 20.0 °C
61.1 µin/in-°F
@Temperature 68.0 °F
ISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 20.0 °C
61.1 µin/in-°F
@Temperature 68.0 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FISO 75-1, 2
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastics Duracon® GH-20 Acetal Co-polymer (POM), GF 20% reinforced, High strength, High rigidity
Polyplastics Tepcon M25 Acetal-copolymer (POM), High Viscosity
Covestro Bayblend® KU 2-1514 Polycarbonate + ABS, Flame Retardant Grade

PPOLPL132 / 57125

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.