MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Morgan Advanced Ceramics Superwool® Plus MD Paper Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Superwool ® Plus MD Paper offers the same benefits of the current Superwool ® fibre family with improved handle ability and enhanced thermal properties. Superwool ® Plus MD Paper is manufactured from pure raw materials using a new proprietary technology. In addition to enhanced thermal properties, large nuisance dust particles have been effectively eliminated making the product less irritating during use.

Typical applications:

  • Industrial and domestic appliance gasketing
  • Glazing applications
  • Passive Fire Protection applications
  • Automotive heat shields

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.230 g/cc0.00831 lb/in³
Loss On Ignition 12 %12 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength <= 0.650 MPa<= 94.3 psiEN 1094-1
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0500 W/m-K
@Temperature 200 °C
0.347 BTU-in/hr-ft²-°F
@Temperature 392 °F
ASTM C201
 0.0700 W/m-K
@Temperature 400 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 752 °F
ASTM C201
 0.110 W/m-K
@Temperature 600 °C
0.763 BTU-in/hr-ft²-°F
@Temperature 1110 °F
ASTM C201
 0.160 W/m-K
@Temperature 800 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 1470 °F
ASTM C201
 0.230 W/m-K
@Temperature 1000 °C
1.60 BTU-in/hr-ft²-°F
@Temperature 1830 °F
ASTM C201
Shrinkage <= 2.0 %
@Treatment Temp. 1000 °C
<= 2.0 %
@Treatment Temp. 1830 °F
 
Descriptive Properties
Classification Temperature (°C)1200
Colorblack/white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6435 / 203219

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.