MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 225-15 MGHU Nylon 6, Glass Fiber/Mineral Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Availability: Asia Pacific; Europe; North America

Fillers/Reinforcement: Glass/Mineral

Uses: Automotive Applications

Automotive Specifications: GM GMP.PA6.001 Color: Black; GM GMP.PA6.001 Color: Natural

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 g/ccASTM D792
Water Absorption 0.70 %
@Time 86400 sec
ASTM D570
Maximum Moisture Content 0.20
Linear Mold Shrinkage, Flow 0.0020 - 0.0035 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 19000 psiASTM D638
Elongation at Break 2.5 %ASTM D638
Elongation at Yield 2.0 %ASTM D638
Flexural Strength 28500 psiASTM D790
Flexural Modulus 1.25e+6 psiASTM D790
Izod Impact, Notched 1.30 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 415 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 407 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 0.762 mm
Oxygen Index 22 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 455 - 485 °F
Middle Barrel Temperature 485 - 505 °F
Front Barrel Temperature 495 - 525 °F
Nozzle Temperature 490 - 515 °F
Melt Temperature 420 °FASTM D789
 485 - 510 °F
Drying Temperature 175 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® B3GM35 BKQ642 23220 15/25% Glass/Mineral Filled PA6 (Conditioned)
Envalior Pocan® B 3235 XF 000000 PBT, 30% Glass Fiber Reinforced
Teknor Apex Chemlon® 225-15 MG Nylon 6, 25% Mineral Reinforced, 15% Glass Fiber Reinforced

PTEKNQ0493 / 236984

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.