MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Thermx® CG923 BK010 PCT
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced

Material Notes: Thermx® CG923 BK010 is a 20% glass fiber reinforced, flame retardant, black polycyclohexylenedimethylene terephthalate resin for injection molding.

Celenese acquired the Thermx product line from DuPont in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.58 g/ccASTM D 792
Density 1.58 g/ccISO 1183
Filler Content 20 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 84ASTM D 785
Tensile Strength at Break 100 MPaISO 527
Tensile Strength, Ultimate 99.0 MPa
@Temperature 23.0 °C
ASTM D 638
Elongation at Break 1.8 %ISO 527
 2.1 %
@Temperature 23.0 °C
ASTM D 638
Tensile Modulus 8000 MPa
@Temperature 23.0 °C
ISO 527
Flexural Strength 140 MPaASTM D 790
 145 MPaISO 178
Flexural Modulus 6750 MPaASTM D 790
 7400 MPaISO 178
Izod Impact, Notched 0.450 J/cm
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Unnotched 430 J/cm
@Temperature 23.0 °C
ASTM D 4812
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 3.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D 257
Surface Resistance 1.00e+16 ohmASTM D 257
Dielectric Constant 3.0
@Frequency 1000 Hz,
Temperature 23.0 °C
ASTM D 150
 3.0
@Frequency 10000 Hz,
Temperature 23.0 °C
ASTM D 150
 3.0
@Frequency 100000 Hz,
Temperature 23.0 °C
ASTM D 150
 3.0
@Frequency 1e+6 Hz,
Temperature 23.0 °C
ASTM D 150
Dielectric Strength 20.7 kV/mm
@Thickness 3.20 mm,
Temperature 23.0 °C
500 V/s, Short Time; ASTM D149
Dissipation Factor 0.0030
@Frequency 100000 Hz
ASTM D 150
 0.0080
@Frequency 1e+6 Hz
ASTM D 150
 0.013
@Frequency 1000 Hz
ASTM D 150
 0.021
@Frequency 10000 Hz
ASTM D 150
 
Thermal PropertiesOriginal ValueComments
Melting Point 283 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 272 °CASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 225 °CISO 75-1/-2
 234 °CASTM D 648
UL RTI, Electrical 150 °C
@Thickness 1.50 mm
UL 746B
 150 °C
@Thickness 3.00 mm
UL 746B
UL RTI, Mechanical without Impact 130 °C
@Thickness 1.50 mm
UL 746B
 130 °C
@Thickness 3.00 mm
UL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
UL94
 V-0
@Thickness 3.00 mm
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
UL94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 300 °COptimum
 295 - 310 °C
Mold Temperature 100 °COptimum
 80.0 - 120 °C
Drying Temperature 95.0 °C
Dry Time 4 - 6 hourDehumidified Dryer
Moisture Content <= 0.030 %
 
Descriptive Properties
ColorBlack
Drying RecommendedYes
FeaturesElectrical Properties, Good
 Flame Retardant
FillerGlass fiber reinforcement
FormsPellets
GenericPCT
Part Marking Code>PCT-GF20FR(17)<ISO 11469
Polymer FamilyPolyester
Polymer TypePCT
Processing MethodInjection Molding
Product CategoryElectrical Resins
 Flame Retardant Resins
 Glass Reinforced Resins
Region AvailableAmericas
 Asia/Pacific
 Europe
Resin IdentificationPCT-GF20FR(17)ISO 1043
UsesConnectors
 E/E Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Thermx® CG023 NC010 PCT
Celanese Thermx® TE1001 BK010 PCT
Celanese Thermx® TE3002 BK010 PCT
Celanese Thermx® CG043 BK010T PCT
Celanese Thermx® CG033 BK010T PCT

PDTA7730 / 89689

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.