MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Viton® A-200 with 30 MT Black and 2.5 VC50 Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Lower viscosity
  • Improved mold flow
  • Excellent extrusion characteristics
  • Better mold release
  • Less mold fouling
  • Improved compression set resistance

Applications

  • Transfer and injection molding for O-rings, Valve stem seals and shaft seals, and Parts with complicated shapes
  • Extrusions for Fuel hose and tubing
  • Solution coating for Fabric and Tanks or chemical containers

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 7724 hours Postcure; ASTM D2240
Tensile Strength at Break 12.4 MPa24 hours Postcure; ASTM D412
Elongation at Break 190 %24 hours Postcure; ASTM D412
100% Modulus 0.00640 GPa
@Strain 100 %
24 hours Postcure; ASTM D412
Compression Set 9.0 %
@Temperature 23.0 °C,
Time 252000 sec
O-Rings; ASTM D395B
 12 %
@Temperature 200 °C,
Time 252000 sec
O-Rings; ASTM D395B
 21 %
@Temperature 232 °C,
Time 79200 sec
O-Rings; ASTM D395B
 21 %
@Temperature 0.000 °C,
Time 252000 sec
O-Rings; ASTM D395B
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 °C
@Time 601 sec
Press Cure
 232 °C
@Time 86400 sec
Postcure
 
Descriptive Properties
Formulation as Tested0.5VPA No.1
 0.5VPA No.3
 2.5Viton® Curative #50
 3MgO
 30MT Black
 6Ca(OH)2
 97.5A-200

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Viton® A-200 with Blanc Fixe Fluoroelastomer Compound
Chemours Viton® A-200 with Celite 350 Fluoroelastomer Compound
Chemours Viton® 40 Process Aid
Chemours Viton® 10 Process Aid
Chemours Viton® A-200 with 45 MT Black and 2.5 VC50 Fluoroelastomer Compound

PDVC9872 / 170513

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.