MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Braskem SVT2180 Renewable Ethylene-Vinyl Acetate Copolymer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: SVT2180 is a copolymer of renewable ethylene with Vinyl Acetate (EVA) mainly used for the production of crosslinked foam sheets and other parts. It is a product with easy processability and high compatibility with mineral fillers, and thermoplastic and elastomeric resins. Other important characteristics are elasticity, flexibility, excellent stress cracking resistance (ESCR), chemical resistance, and low temperature strength. The exclusive morphologic characteristics give an outstanding crosslinkability. The components produced with SVT2180 have the following properties: low weight, resistance to deformation, low shrink, high capacity of sticking and color retention.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D1505 / ASTM D792
Vinyl Acetate Content 19 %ASTM D5594-98
Melt Flow 2.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 89ASTM D2240
Hardness, Shore D 38ASTM D2240
Tensile Strength at Break 19.0 MPaASTM D638
Elongation at Break 750 %ASTM D638
Secant Modulus 0.0330 GPa5% Secant Modulus; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 86.0 °CASTM D3418
Vicat Softening Point 61.0 °C
@Load 1.02 kg
ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBRAS602 / 313995

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.