Polycarbonate / polyester alloy (special fine filament). Availability: Africa, Middle East, Asia Pacific, Europe, Latin America, North America. Features: Chemical resistant, high rigidity, good surface finish, UV resistant. Uses: Handles. Forms: pellets. Processing Method: Injection Molding.Information provided by Teijin Chemicals Ltd. |