Excellent Barrier Performance, Medium Impact/Stiffness. HYPERIER is a nano compound made from nano-sized inorganic plate clay. Application: 5L~20L: Agrochemical Container, SORE Fuel Tank, PFC CAS No. 25750-23-6 and 9002-88-4 Information provided by LG Chemical |