MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Hytrel® 6359FG NC010 TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 63 Shore D High Performance Polyester Elastomer Developed for Food Contact Applications

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccISO 1183
Melt Density 1.04 g/cc
@Temperature 240 °C
Water Absorption 0.60 %
@Thickness 2.00 mm
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.015 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.015 cm/cmISO 294-4, 2577
Melt Flow 8.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
cm³/10min Volumetric; ISO 1133
 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 5815s; ISO 48-4
 <= 63ISO 48-4
Tensile Stress at Strain 12.0 MPa
@Strain 5.0 %
1BA specimen at 50mm/min; ISO 527-1/-2
 15.0 MPa
@Strain 10 %
ISO 527-1/-2
Tensile Modulus 260 MPaISO 527-1/-2
Poissons Ratio 0.48
Izod Impact, Notched (ISO) 19.0 kJ/m²
@Temperature -40.0 °C
ISO 180/1A
 81.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 25.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 110 kJ/m²
@Temperature 23.0 °C
Partial Break; ISO 179/1eA
Tear Strength 158 kN/mparallel; ISO 34-1
 174 kN/mnormal; ISO 34-1
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 2.16 J/g-°C
@Temperature 240 °C
Melt
Thermal Conductivity 0.140 W/m-K
@Temperature 240 °C
Melt
Melting Point 211 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CISO 75-1/-2
Vicat Softening Point 100 °C50°C/h, 50N; ISO 306
 195 °C50°C/h 10N; ISO 306
Brittleness Temperature -100 °CISO 974
Glass Transition Temp, Tg -5.00 °C10°C/min; ISO 11357-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 °COptimum, Extrusion
 225 - 240 °CRange, Extrusion
 240 °COptimum, Injection
 235 - 260 °CRange, Injection
Mold Temperature 45.0 °COptimum, Injection
 45.0 - 55.0 °CInjection
Drying Temperature 100 °CInjection
 90.0 - 110 °CExtrusion
Dry Time 2.00 - 3.00 hourExtrusion, Dehumidified Dryer
 2.00 - 3.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.060 %Extrusion
 <= 0.080 %Injection
Hold Pressure <= 70.0 MPaInjection
 
Descriptive Properties
Drying RecommendedyesInjection
Eff. thermal diffusivity (m²/s)5.44E-08
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging (mg)0.1G-value (condensate); ISO 6452
Odor Class2.5VDA 270
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Resin IdentificationTPC-ETISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hytrel® HTR8068 TPC-ET-FR(17)
Celanese Hytrel® HTR8223 BK320 TPC-ET
Celanese Hytrel® HTR8341C BK320 TPC-ET
DuPont Mobility and Materials Hytrel® HTR8136BK TPC-ET
DuPont Mobility and Materials Hytrel® HTR8139BK TPC-ET

PDSX5188 / 197828

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.