MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC SABIC® Vestolen A 6060R 10000 Black PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: SABIC® Vestolen A 6060R 10000 (black) is a grade which has a high density and a bimodal distribution of the molecular mass. Due to its profile of properties this material is typically used for gas, drinking water and waste water piping. This material meets (inter)national standards for use in gas, drinking water and waste water piping. MRS class ISO 12162 MPa = 10.0 (PE 100). This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.959 g/ccASTM D1505
Oxidative Induction Time (OIT) >= 20 min
@Temperature 210 °C
ISO 11357-6
Carbon Black Loading 2.25 %ISO 6964
Melt Flow 0.10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 0.30 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 59ISO 868
Tensile Strength, Yield 24.0 MPaTest specimen according to ISO 527-2 type 1BA, thickness 2 mm,Speed of testing: 50 mm/min; ISO 527-2
Elongation at Yield 9.0 %Test specimen according to ISO 527-2 type 1BA, thickness 2 mm,Speed of testing: 50 mm/min; ISO 527-2
Tensile Modulus 1050 MPaTest specimen according to ISO 527-2 type 1BA, thickness 2 mm,Speed of testing: 50 mm/min; ISO 527-2
Charpy Impact, Notched 9.20 kJ/m²ISO 179/1eA
 23.0 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 124 - 128 °CDIN 53765
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °CISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 43.0 °CISO 75-2
Vicat Softening Point 71.0 °Cat 50 N (VST/B); Conditioning of test specimen: temp. 23 °C, relative humidity 50 %, 24 hours; ISO 306
 
Descriptive Properties
ColorBlack
MRS classification10 MPaISO 12162
RAL number9004

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11114 / 244581

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.