Notes: Monprene CP-37968 is a general purpose thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-37968 is a medium density, medium hardness, filled grade, available in NAT, BLK, and colors and is suitable for injection molding and extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Filled; Light Stabilized; Lubricated; Medium Flow; Medium Hardness; Medium Density Uses: Consumer Applications; Gaskets; General Purpose; Handles; Tubing RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |