MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
436 Stainless Steel annealed bar
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 400 Series Stainless Steel

Key Words: UNS S43600, SAE J405 (51436)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 155
Hardness, Knoop 175Converted from Brinell
Hardness, Rockwell B 82Converted from Brinell
Hardness, Vickers 162Converted from Brinell
Tensile Strength, Ultimate 517 MPa
Tensile Strength, Yield 310 MPa
@Strain 0.2 %
Elongation at Break 30 %in 50 mm
Modulus of Elasticity 200 GPa
 200 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000600 ohm-cm
 0.0000600 ohm-cm
@Temperature 20.0 °C
Magnetic Permeability 600 - 1100annealed condition at RT
 600 - 1100
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.4 µm/m-°C
@Temperature 0.000 - 100 °C
 11.0 µm/m-°C
@Temperature 0.000 - 315 °C
 11.3 µm/m-°C
@Temperature 0.000 - 540 °C
 11.9 µm/m-°C
@Temperature 0.000 - 650 °C
 12.4 µm/m-°C
@Temperature 0.000 - 815 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 23.9 W/m-K
@Temperature 100 °C
 26.0 W/m-K
@Temperature 500 °C
 26.1 W/m-K
@Temperature 100 °C
 26.3 W/m-K
@Temperature 500 °C
Melting Point 1425 - 1510 °C
 1425 - 1510 °C
Solidus 1425 °C
 1425 °C
Liquidus 1510 °C
 1510 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.12 %
Chromium, Cr 14 - 18 %
Iron, Fe 78 - 84.9 %as balance
Manganese, Mn <= 1.0 %
Molybdenum, Mo 0.75 - 1.25 %
Nb + Ta 0.40 - 0.60 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
434 Stainless Steel annealed bar
435 Stainless Steel annealed bar
420 Stainless Steel, annealed bar
430 Stainless Steel annealed bar
434 Stainless Steel annealed sheet

MQ436S / 13211

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.