MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BYK ADD-MAX® AF 488 Antifog masterbatch on LLDPE/EVA carrier  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Ethylene Vinyl Acetate; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Fields of application: Extruded films and sheets from LDPE or LLDPE.

Examples: Food wrap films.

Mode of action and advantages: ADD-VANCE AF 488 contains a very effective antifogging additive. The antifog additive in ADD-VANCE AF 488 reduces formation of water droplets on plastic surfaces and as a result improves the transparency of the film or sheet.

Advantages: Excellent results in cold and hot fog tests; Improved transparency of the sheet/film; Non-sticking granules; and Safe and easy handling, dust free.

Regulations: ADD-VANCE AF 488 is very suitable for food packaging products as the active ingredients are in compliance with current food contact regulations.

Former ADDCOMP product line, acquired by BYK.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 250 °C
 
Descriptive Properties
AppearanceWhite/off-white granules
Dosing Level3-5%

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® OB13AF Polyester Film, 100 Gauge
BYK ADD-VANCE® FR 825 EVA based flame-retardant masterbatch
A. Schulman POLYBATCH™ AF-1085 Antifog Concentrate
Innospec FLEXAREN® 14006 EVA-Copolymer
Innospec FLEXAREN® 14003 EVA-Copolymer

PPADDC41 / 133254

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.