MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Redwood Plastics Redco™ CG-SS80 Sheet Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Commercial Grade silicone sheeting is designed to be used in applications where physical properties are not critical but extreme temperature resistance and reliable performance are still needed. Silicone rubber has the combined properties of resilience, high temperature stability, and general inertness unavailable in any other elastomer. Silicones are generally unaffected by extended exposure to temperatures from -75º up to +232ºF and are also resistant to aging and degradation from sunlight and ozone. Silicone is a polysiloxane chain. Unlike other rubbers, its molecular matrix does not contain carbon, but consists of silicone and oxygen atoms. It can be formulated to achieve flame resistance, electrical or thermal conductivity, electrostatic dissipative (ESD) as well as FDA and medical compliance.

Typical Applications:

  • High temp seal and gaskets
  • Wipers & squeegees
  • Electrical Insulators
  • FDA approved applications
  • Digital print roller covers
  • O-rings
Core Advantages:
  • Exceptional high & low temperature resistance
  • Unaffected by ozone, weather and UV radiation
  • Good electrical insulator
  • Self-extinguishable
  • Maintains a stable shore hardness and consistant physical properties through wide temperature range

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 73 - 8773 - 87ASTM D 2240
 78 - 82
@Temperature >=70.0 °C,
Time 360000 sec
78 - 82
@Temperature >=158 °F,
Time 100 hour
Accelerated Aging @ 30% RH; ASTM D 1056
Tensile Strength 6.07 MPa880 psiASTM D 412
 8.191 MPa
@Temperature >=70.0 °C,
Time 360000 sec
1188 psi
@Temperature >=158 °F,
Time 100 hour
Accelerated Aging @ 30% RH; ASTM D 1056
Elongation at Break 300 %300 %ASTM D412
 390 %
@Temperature >=70.0 °C,
Time 360000 sec
390 %
@Temperature >=158 °F,
Time 100 hour
Accelerated Aging @ 30% RH; ASTM D 1056
Compression Set 10 %10 %ASTM D 395 Method B
 
Descriptive Properties
Bonding Strength>7 N.mm-1Bond Between Steel and Elastomer Laminae, ASTM D 429, Method B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREDW089 / 296655

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.