MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Crystalbond™ 555-HMP Washaway Mounting Adhesive & Accessory
Categories: Polymer; Adhesive

Material Notes: Low melting point adhesive systems for moderate-stress machining processes, dry plasma etching of silicon wafers and de-paneling copper plated Teflon boards. Transparent in thin cross-sections. Soluble in hot water.

Vendors: Aremco’s Crystalbond and Wafer-Mount products are ideal for temporarily mounting ceramics, glass, quartz, and semiconductor substrates for dicing and polishing operations. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 250 cP
@Temperature 116 °C
#3 Spindle @30 RPM
 500 cP
@Temperature 88.0 °C
#3 Spindle @30 RPM
 1000 cP
@Temperature 68.0 °C
#3 Spindle @30 RPM
 2000 cP
@Temperature 54.0 °C
#3 Spindle @30 RPM
 2800 cP
@Temperature 49.0 °C
#3 Spindle @30 RPM
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 335 psi
 
Thermal PropertiesOriginal ValueComments
Melting Point 66.0 °CFlow Point
 
Descriptive Properties
Available FormsStick, 1/2” × 1” × 7”
ColorWhite
SolventHot Water
Weight0.15 Lbs/Stick

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Indium Corp. Indalloy® 228 Pb-Sn-Ag Solder Alloy

PAREM33 / 24297

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.