MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled BK 15045 PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled

Material Notes: Description: Easy flowing injection molding grade with 15 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg timer dials, toggles, knobs, parts for thermostats, oven-door handles, toaster housings and grills)

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.600 - 0.900 g/cc
Density 1.41 g/ccISO 1183
Water Absorption 0.40 %ISO 62
Moisture Absorption at Equilibrium 0.20 %ISO 62
Viscosity Test 100 cm³/gISO 307
Linear Mold Shrinkage, Flow 0.0070 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cmISO 2577
Melt Flow 35.25 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPaISO 527-1/-2
Elongation at Break 3.5 %ISO 527-1/-2
Tensile Modulus 5500 MPaISO 527-1/-2
Charpy Impact Unnotched 30.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 5.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Dielectric Constant 3.7
@Frequency 1e+6 Hz
IEC 60250
 3.7
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0012
@Frequency 100 Hz
IEC 60250
 0.015
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 300 VTest Solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 223 °CISO 11357-1/-2
Maximum Service Temperature, Air 210 °C
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °CISO 75-1/-2
Decomposition Temperature >= 290 °C
Flammability, UL94 HB
@Thickness 1.60 mm
Ignition Temperature 350 °CASTM D1929
 
Processing PropertiesOriginal ValueComments
Melt Temperature 203 - 275 °CInjection molding/Extrusion
Mold Temperature 60.0 - 100 °CInjection molding
 
Descriptive Properties
ColorBK 15045
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® B 4300 G3 15% Glass Filled PBT
BASF Ultradur® B 4300 G2 10% Glass Filled PBT
BASF Ultradur® B 4500 PBT
BASF Ultradur® B 4300 G6 30% Glass Filled PBT
Samyang Tribit® 1503S Polybutylene Terephthalate

PBASG0125 / 131758

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.