Features: Characteristics : Good balance of toughness & stiffness stress Additives : Anti-Oxidants, Lubricants Processing recommendations : Maintain the stock temperature 200-230°C (392-446°C) for optimum part qualityApplication: Utilized electrical conduit, corrugated pipe CAS No. 25213-02-9 Information provided by LG Chemical |