MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Dyneon™ PVDF 1010/0001 Polyvinylidene Fluoride  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, and oil and gas industry, PVDF is also gaining recognition in automotive, building, electronics, pharmaceutical and batteries. 3M™ Dyneon™ PVDF 1010/0001 is easily processed under a variety of conventional thermoplastic conversion techniques, being particularly suitable for extrusion. PVDF 1010/0001 is inherently pure and chemically resistant against a variety of aggressive fluids and solvents. PVDF 1010/0001 exhibits excellent dimensional stability, abrasion resistance and high strength, and maintains its mechanical properties at elevated temperature.
  • Excellent chemical resistance to a variety of aggressive fluids and solvents
  • Good permeation resistance
  • Extrusion grade
  • Excellent strength and dimensional stability

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.78 g/cc0.0643 lb/in³ISO 1183
Water Absorption <= 0.040 %<= 0.040 %24 hr @ 23°C; ISO 62 (method 1)
Melt Index of Compound  2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 6.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
6.0 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 42.0 MPa6090 psiASTM D638
Tensile Strength, Yield 55.0 MPa7980 psi50mm/min; ASTM D638
Elongation at Break 35 %35 %ASTM D638
Elongation at Yield 7.0 %7.0 %50mm/min; ASTM D638
Flexural Modulus 2.10 GPa305 ksi2mm/min; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 174 °C345 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 147 °C297 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 113 °C235 °F
Flammability, UL94 V-0V-0
Oxygen Index >= 44 %>= 44 %ASTM D2863
 
Descriptive Properties
FormGranules

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Chemours Teflon® FEP 5100 Fluoropolymer Resin
Arkema Kynar® 705 PVDF
Arkema KYNAR® 6000 HD Polyvinylidene Fluoride - Injection Molding
Arkema KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion

PDYNE056 / 34864

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.