MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Trigonox 121-C75 Acrylics tert-Amyl peroxy-2-ethylhexanoate
Categories: Other Engineering Material

Material Notes: Trigonox 121-C75 is an initiator (75% active ingredient in odorless mineral spirits) for (co)polymerization of acrylates and methacrylates.

CAS number: 686-31-7

EINECS/ELINCS No: 211-687-3

Applications: Polymerization of ethylene: Trigonox 121-C75 may be used for the polymerization of ethylene at high pressure in both autoclave and tubular processes. To obtain a wide spectrum of polymerization temperatures, Trigonox 121-C75 may be used in combination with other peroxides. Trigonox 121-C75 is suitable for use in curing unsaturated polyester, vinyl ester and acrylic thermosetting resins in the temperature range of 80 – 130°C (176 – 266°F). Trigonox 121-C75 offers greater reactivity than Trigonox 21, and finds use in a variety of applications including pultrusion, molding compounds and curedin- place pipe systems. It is also an effective finishing initiator for use in ambient cured systems to lower residual monomer content and improve cure.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Half-life  0.100
@Temperature 111 °C
0.100
@Temperature 232 °F
[hr]
 1.00
@Temperature 91.0 °C
1.00
@Temperature 196 °F
[hr]
 10.0
@Temperature 73.0 °C
10.0
@Temperature 163 °F
[hr]
Molecular Weight 230.3 g/mol230.3 g/mol
Storage Temperature <= 10.0 °C<= 50.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 35.0 °C95.0 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
Content (%)6.95Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY995 / 286518

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.