MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Tisan TISBLEND® PC/ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: TISBLEND has a wide area of application in electric/electronic, food packaging, information technology, information technology, medical and automotive industries. General Specification include:
  • High impact resistance
  • Toughness
  • Dimensional stability
  • Excellent surface quality
  • High temperature endurance
  • Easy processability
They have excellent chemical resistance to weak acids. They have good resistance to strong acids and weak alkalis. They have medium resistance to strong alkalis. They have weak resistance to organic solvents, alcohols, hydrocarbons, and engine fuels.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 - 270 °C
 
Processing PropertiesOriginal ValueComments
Feed Temperature 70.0 °C
Rear Barrel Temperature 220 - 230 °CAft-1. Region Temperature
Middle Barrel Temperature 225 - 235 °CMid-2. Region Temperature
Front Barrel Temperature 230 - 240 °CPre-3. Region Temperature
Nozzle Temperature 250 - 265 °C
Melt Temperature 220 - 270 °C
Drying Temperature 90.0 - 120 °CPredrying Temperature
Dry Time 3 - 5 hourPredrying Time
 
Descriptive Properties
Block Temperature70°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cossa Polimeri ESTADIENE 4009 Acrylonitrile Butadiene Styrene
Ineos ABS Lustran® M205FC ABS Pellets, Injection Molding Grade
Nexeo® HIVAL® 62408 Acrylonitrile Butadiene Styrene
INEOS Styrolution Lustran® 620 Acrylonitrile Butadiene Styrene (ABS)
Ineos ABS Lustran® QE 1030, Extrusion Grade

PTIS064 / 79499

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.