MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LyondellBasell Hostalen PP H1022 12 Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Hostalen PP H1022 12 is a black colored polypropylene block copolymer with high melt viscosity and good low-temperature impact strength. The product is typically used in the application injection molded fittings. Applications: Fittings, Industrial, Soil & Waste Pipe

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.908 g/cc0.0328 lb/in³ISO 1183-1
Melt Flow  0.30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 0.50 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.50 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 1.3 g/10 min
@Load 5.00 kg,
Temperature 230 °C
1.3 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464ISO 868
Ball Indentation Hardness 50.0 MPa7250 psiISO 2039-1
Tensile Strength, Yield 31.0 MPa4500 psiISO 527-1,-2
Elongation at Yield 12 %12 %50mm/min; ISO 527-1,-2
Tensile Modulus 1.40 GPa203 ksiISO 527-1,-2
Charpy Impact, Notched  0.700 J/cm²
@Temperature -20.0 °C
3.33 ft-lb/in²
@Temperature -4.00 °F
ISO 179
 2.10 J/cm²
@Temperature 0.000 °C
9.99 ft-lb/in²
@Temperature 32.0 °F
ISO 179
 11.7 J/cm²
@Temperature 23.0 °C
55.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C196 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 75.0 °C167 °FB50N; ISO 306
 158 °C316 °FA50; ISO 306
DSC Induction Temperature 164 °C327 °FISO 3146
 
Descriptive Properties
Ball Indentation Hardness (MPa)H 132/30
Processing Methodinjection molding, pipe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene Copolymer
LyondellBasell Pro-fax™ RP320N Polypropylene Copolymer
LyondellBasell Moplen EP548U Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Hostalen PP H1850 Polypropylene Copolymer
LyondellBasell Hostacom DYS 707N E G82764 Polypropylene Copolymer

PEQT8504 / 220139

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.