MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Accella Bayblock® Prime EW Epoxy primer
Categories: Polymer; Thermoset; Epoxy

Material Notes: Characterization: Bayblock Prime EW is a two-component, water-based epoxy primer.

Properties / Applications: Bayblock Prime EW is a multi-purpose, thixotropic, easy spreading primer. Bayblock Prime EW adheres well to most metals, organic polymers, wood, masonry and vitreous surfaces. It may also be used as masonry block filler. It should not be used on copper or silver. Bayblock Prime EW cures to form a solvent and vapor resistance film. Bayblock Prime EW has excellent alkali resistance, good solvent resistance, fair acid resistance and poor chalk resistance. It is not intended for continuous exterior use. Bayblock Prime EW cures to form a hard, lusterless coating. As with any product, use of Bayblock Prime EW in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Covestro sold their spray polyurethane foam business to Accella in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 40.5 - 44.5 %40.5 - 44.5 %ASTM D2697, by volume
 58 - 62 %58 - 62 %ASTM D1644, by weight
Volatile Organic Compounds (VOC) Content <= 55 g/l<= 55 g/l
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.2 °C180 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flash Point >= 100 °C>= 212 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0063 / 201846

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.