Hostacom CA199P NATRL low melt flow, 400 MPa flexural modulus thermoplastic elastomeric olefin (TEO) resin exhibits balanced strength, toughness, flexibility and ductility. It is typically used for mold-in color interior automotive applications. Applications: Automotive Parts, Interior Automotive Applications.Information provided by LyondellBasell. |