MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Novec™ 612 Magnesium Protection Fluid
Categories: Fluid

Material Notes: Novec 612 fluid, dodecafluoro-2-methyl-3-pentanone or (CF3CF2C(O)CF(CF3)2, is a clear, colorless, and low odor fluid. Its properties, environmental profile, and margin of safety make it a sustainable material for protecting molten reactive metals such as magnesium and its alloys. Novec 612 fluid has the advantage of being a liquid at room temperature. This makes it easy to transport in conventional liquid containers of all sizes. Because of its low viscosity, Novec 612 fluid also is easy to transfer by pumping. Yet it quickly and easily evaporates into a gas stream for use as a cover gas because of its high vapor pressure and low heat of vaporization

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/ccSat. Liquid
 0.0136 g/cc
@Pressure 0.101 MPa
Gas
Viscosity Measure 0.39 cStLiquid
Molecular Weight 316.04 g/mol
Vapor Pressure 0.404 bar
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 18.65 bar
Critical Temperature 168.7 °C
Critical Density 0.639 g/cc
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 88.0 J/gat boiling point
Specific Heat Capacity 1.103 J/g-°CLiquid
 0.891 J/g-°C
@Pressure 0.101 MPa
Vapor
Boiling Point 49.2 °C
@Pressure 0.101 MPa
 
Descriptive Properties
Relative Dielectric Strength2.31 atm (N2=1.0)
Solubility of Water<0.001%in Novec 612 Fluid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Fluorinert™ FC-72 Electronic Liquid
3M Novec™ 1230 Fire Protection Fluid
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (31 wt% - 36 wt% Concentration)
Solvay Chemicals 38% Technical Grade Hydrochloric acid
LG Chemical c-Pentane

PMM33092 / 167839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.