MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kumho-Sunny HU650Z ABS, Heat Resistance
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes: ABSHU650Z is heat resistance ABS with low gloss, high rigidity, toughness and good UV stability.

Application: Hair dryer shells, electric oven exterior parts and microwave ovens etc.

Features: Low Gloss; High Rigidity

Information provided by Shanghai Kumho Sunny Plastics co, Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ISO 1183
Maximum Moisture Content 0.0500.050
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inISO 294
Melt Flow 5.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
5.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ISO 2039-2
Tensile Strength, Yield 45.0 MPa6530 psi50mm/min; ISO 527
Elongation at Break 10 %10 %50mm/min; ISO 527
Flexural Strength 62.0 MPa8990 psi2mm/min; ISO 178
Flexural Modulus 2.20 GPa319 ksi2mm/min; ISO 178
Poissons Ratio 0.400.401mm/min; ISO 527
Izod Impact, Notched (ISO)  6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
5.5J; ISO 180
 12.0 kJ/m²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
5.5J; ISO 180
Izod Impact, Unnotched (ISO) 65.0 kJ/m²30.9 ft-lb/in²5.5J; ISO 180
Charpy Impact Unnotched 7.00 J/cm²33.3 ft-lb/in²4J; ISO 179
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
4J; ISO 179
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
4J; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C216 °F120°C/h; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C198 °F120°C/h; ISO 75
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 220 - 240 °C428 - 464 °F
Middle Barrel Temperature 230 - 250 °C446 - 482 °F
Front Barrel Temperature 240 - 260 °C464 - 500 °F
Nozzle Temperature 250 - 270 °C482 - 518 °F
Melt Temperature 240 - 260 °C464 - 500 °F
Mold Temperature 50.0 - 80.0 °C122 - 176 °F
Drying Temperature 90.0 - 105 °C194 - 221 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
 
Descriptive Properties
Flammability=80 mm/min355×100×3 mm, ISO 3795

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKMSN036 / 280888

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.