A soft, special purpose supplementary resin with a wide compatibility range, designed to improve the initial, long-term and intercoat adhesion of paints based on vinyl chloride copolymers and in a number of other binders to metallic and mineral substrates and to certain plastics. Depending on the binder, it also improves the flexibility at normal and low temperatures |