MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LEXAN™ FR LUX9610 PC (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN LUX9610 is an injection moldable polycarbonate (PC) with an MVR (300°C/1.2kg) 7. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0@1.5mm rating. This is a UV stabilized, transparent grade with high optical clarity and impact resistance.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Density 1.07 g/cc0.0387 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inSABIC method
Melt Flow 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.0 MPa9430 psi50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPa8990 psi50 mm/min; ASTM D638
Elongation at Break 110 %110 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %6.0 %50 mm/min; ASTM D638
Tensile Modulus 2.32 GPa336 ksi50 mm/min; ASTM D638
Flexural Yield Strength 95.0 MPa13800 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.30 GPa334 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 7.60 J/cm14.2 ft-lb/inASTM D256
 1.23 J/cm
@Temperature -30.0 °C
2.30 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched NBNBASTM D4812
Dart Drop, Total Energy 75.0 J55.3 ft-lbpeak; ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec15 - 30 secUL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs60 - 120 arcsUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
37.8 µin/in-°F
@Temperature -40.0 - 203 °F
ASTM E831
CTE, linear, Transverse to Flow 68.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
37.8 µin/in-°F
@Temperature -40.0 - 203 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 142 °C
@Thickness 3.20 mm
288 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
@Thickness 3.20 mm
257 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 145 °C293 °FRate B/120; ISO 306
UL RTI, Electrical 125 °C257 °FUL 746B
UL RTI, Mechanical with Impact 115 °C239 °FUL 746B
UL RTI, Mechanical without Impact 125 °C257 °FUL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 275 - 300 °C527 - 572 °FInjection Molding
Zone 1 260 - 280 °C500 - 536 °F
Zone 2 270 - 295 °C518 - 563 °F
Zone 3 280 - 305 °C536 - 581 °F
Melt Temperature 280 - 305 °C536 - 581 °F
Mold Temperature 70.0 - 95.0 °C158 - 203 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 48.0 hour48.0 hourCumulative; Injection Molding
Moisture Content 0.020 %0.020 %
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10645 / 244112

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.