MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Petroquimica Triunfo Trithene® TS 7003 LDPE - High Strength Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: The Trithene® TS 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily processed and allows high thickness uniformity. The product was developed to meet the requirements for automatic packaging: good clarity, productivity, low coefficient of friction (COF) and sealability. Trithene® TS 7003 resin shows excellent performance in conventional extruders and low energy consumption during processing. This product complies with ASTM standard D1248-IA5 and the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.

Applications: Films for automatic packaging of liquids, such as milk, yogurt, juices, etc. Packaging for frozen food: meat, chicken, seafood, fries, etc.

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Key Words: FDA: 21 CFR 177.1520 (C) 2.1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.922 - 0.924 g/ccASTM D1505
Thickness 50.0 microns
Melt Index of Compound 0.23 - 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 17.0 MPaASTM D638
Tensile Strength, Yield 11.0 MPaASTM D638
Film Elongation at Break, MD 300 %ASTM D882
Film Elongation at Break, TD 625 %ASTM D882
Elongation at Break 585 %ASTM D638
Secant Modulus, MD 0.115 GPa5%; ASTM D882
Secant Modulus, TD 0.125 GPa5%; ASTM D882
Coefficient of Friction, Dynamic 0.15ASTM D1894
Elmendorf Tear Strength, MD 6.00 g/micronASTM D1922
Elmendorf Tear Strength, TD 4.60 g/micronASTM D1922
Dart Drop Test 190 g(method A); ASTM D1709
Film Tensile Strength at Break, MD 27.0 MPaASTM D882
Film Tensile Strength at Break, TD 23.5 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 94.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 18 %ASTM D1003
Gloss 64 %@ 60° Gardner; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 165 - 175 °CPlasticizing Zone
 170 - 190 °CMixture Zone
Feed Temperature 160 - 170 °C
Adapter Temperature 185 - 200 °C
Blow-up Ratio (BUR) 3.0Recommended
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film
Dow DOWLEX™ 2245A Linear Low Density Polyethylene, Heavy Duty Film Grade
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade
Braskem LD5000A LDPE Blow Molding Polyethylene
Braskem EG0921 LDPE Blow Molding Polyethylene

PDAX085 / 29510

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.