MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 2099 X 134682 Polycarbonate/PBT Alloy; Permanently Static Dissipative - ESD Protection - Impact Modified - UV Stabilized
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: This compound has been formulated to meet the static dissipative requirements of the ATEX Directive.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccASTM D 792
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
@Thickness 3.20 mm
ASTM D 955
Melt Flow 5.0 - 8.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 6000 psiASTM D 638
Elongation at Break >= 10 %ASTM D 638
Tensile Modulus 240 ksiASTM D 638
Flexural Strength 9500 psiASTM D 790
Flexural Modulus 250 ksiASTM D 790
Izod Impact, Notched 14.0 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Surface Resistance <= 1.00e+9 ohmESD STM11.11
Static Decay <= 0.50 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 205 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 183 °FASTM D 648
Flammability, UL94 HB
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 410 - 480 °F
Mold Temperature 150 - 230 °F
Drying Temperature 180 °F
@Time 14400 sec
Moisture Content <= 0.020 %
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Molded
RTP Company RTP 201 UV Nylon 6/6 (PA), Glass Fiber - UV Stabilized
Avient Edgetek® XT XT-100-BU01-HF Polycarbonate + PBT (PC+PBT)
Envalior Pocan® DP C 1502 000000 PBT+PC
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP

PQZRA26536 / 206034

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.