TRA-BOND 516H01 is a room temperature curing, low viscosity adhesive formulated for terminating ALL TYPES of fiber optic connectors, including Pre-Mixed and Frozen applications. It has also been used for bonding LED displays, lenses and other optical components. TRA-BOND 516H01 provides both high bond strength as well as low stress connections with no pistoning. TRA-BOND 516H01 is provided in a dark blue color to allow easy polishing. Information provided by Tra-Con Inc. |