MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® TRVX-50X9 nat PAMACM12-GF50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, 50% Glass Fiber Filled

Material Notes: Product description: Grilamid TRVX-50X9 is a 50% glass fiber reinforced amorphous polyamide. This product shows a very low tendency of distortion and is therefore especially suitable for complex and thin walled designs. It offers a variety of interesting properties such as:
  • High stiffness and strength
  • Good impact resistance
  • Very low distortion
  • Minor sink mark tendency
  • Low flash tendency
  • High dimensional stability
  • Low moisture absorption
  • Easy processing with good melt flow
Grilamid TRVX-50X9 can be used for applications in:
  • Electrical / Electronics
  • Telecommunication
  • Construction / Industry

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccDry; ISO 1183
Water Absorption 1.0 %Sim. to ISO 62
Moisture Absorption 0.300 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0010 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 190 MPaConditioned; ISO 2039-1
Tensile Strength at Break 160 MPaConditioned; ISO 527-1/-2
Elongation at Break 2.1 %Conditioned; ISO 527-1/-2
Tensile Modulus 12500 MPaConditioned; ISO 527-1/-2
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 65.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 16.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 32.0 kV/mmConditioned; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°CISO 11359-1/-2
Maximum Service Temperature, Air 80.0 - 110 °CLong Term; ISO 2578
 120 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 115 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 105 °CISO 75-1/-2
Glass Transition Temp, Tg 125 °C10°C/min; ISO 11357-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Cooling and climate control
 Powertrain and Chassis
Electricals & ElectronicsElectrical appliances
 Electrical equipment
 Energy distribution
 Mobile phones and other portable devices
FormGranules
Industry & Consumer goodsHeating systems
 Housewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Medical devices
 Power transmission
 Tools & Accessories
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teijin Panlite® LV-2225ZS Polycarbonate
EMS-Grivory Grilamid® LV-65H FWA nat PA12-GF65
EMS-Grivory Grilamid® LV-3A H PA12-GF30
EMS-Grivory Grilamid® LV-30H FWA black 9225 PA12-GF30
EMS-Grivory Grilamid® L 20 G PA12

PGRH111 / 156820

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.