MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Envision™ 480Cv3 Print Wrap Film
Categories: Polymer; Film

Material Notes: High performance, 2-mil white, non-PVC film with a luster finish; Pressure-act adhesive for easy sliding, tacking, snap up and repositioning; non-visible air release channels for fast and easy, bubble-free installations; For inkjet printing with select solvent, eco-solvent, UV and latex inks and for screen priming with select solvent and UV inks. Refer to the Compatible Products and Warranty information sections for the recommended printing platforms; Versatile, ideal for many long-term graphic applications and for short-term wall graphics on smooth or moderately textured surfaces; Flexible, highly conformable over compound curves, corrugations and rivets and requires less heat during application than vinyl films – Stretch graphic construction using selected inks with the 3M™ Envision™ Gloss Wrap Overlaminate 8548G up to 150% ( for example, a 10 inch piece of film can stretch to 15 inches) without primer or relief cuts while maintain lifting resistance; see details and exceptions in Section 9; Removable film, resists tearing in cooler temperature for fast removal; Non-PVC, phthalate-free film; Contains no added chlorine or halogens; Made in part from bio-based materials; Manufactured using 60% less solvent

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 2.00 milwithout adhesive
 3.00 - 4.00 milwith adhesive
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 37.9 - 44.8 MPa
Peel Strength 2.00 - 4.00 pliAdhesion to ABS
 2.00 - 4.00 pliAdhesion to Acrylic enamel
 2.00 - 4.00 pliAdhesion to Fruehauf pre-painted panels
 3.00 - 5.00 pliAdhesion to Automotive clear coats
 4.00 - 6.00 pliAdhesion to Aluminum, etched
 5.00 - 7.00 pliAdhesion to Aluminum, anodized
 
Processing PropertiesOriginal ValueComments
Processing Temperature 4.00 - 38.0 °CApplication Temp; Flat without rivets
 4.00 - 38.0 °CApplication Temp; Walls
 16.0 - 32.0 °CApplication Temp; Compound Curves and/or watercraft
 10.0 - 38.0 °CApplication Temp; Curves or corrugations with rivets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM34828 / 169575

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.