MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® RG-12160 XRD1 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene RG-12160 XRD1 is specifically designed for food contact applications and other regulated markets such as children’s and infants products. Monprene RG-12160 XRD1 is a low density, medium hardness grade that is suitable for injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Low Density; Medium Flow; Low Specific Gravity; Medium Hardness; Lubricated; Slip; Without Fillers

Uses: Consumer Applications; Gaskets; Handles; Kitchenware; Safety Equipment; Sporting Goods; Toothbrush Handles; Toys; Tubing; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccASTM D792
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60
@Time 5.00 sec
Injection Molded; ASTM D2240
 62
@Time 1.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 755 psiDie C, 20 in/min, Flow; ASTM D412
 984 psiDie C, 20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain 254 psi
@Strain 100 %
Die C, 20 in/min, Across Flow; ASTM D412
 415 psi
@Strain 300 %
Die C, 20 in/min, Across Flow; ASTM D412
 556 psi
@Strain 100 %
Die C, 20 in/min, Flow; ASTM D412
 666 psi
@Strain 300 %
Die C, 20 in/min, Flow; ASTM D412
Elongation at Break 390 %Die C, 20 in/min, Flow; ASTM D412
 650 %Die C, 20 in/min, Across Flow; ASTM D412
Tear Strength 129 pliDie C, 20 in/min, Flow; ASTM D624
 178 pliDie C, 20 in/min, Across Flow; ASTM D624
Compression Set 24 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ASTM D395B
 44 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ASTM D395B
 
Processing PropertiesOriginal ValueComments
Processing Temperature 356 - 446 °FMelt, Injection
Rear Barrel Temperature 356 - 446 °FInjection
Middle Barrel Temperature 356 - 446 °FInjection
Front Barrel Temperature 356 - 446 °FInjection
Nozzle Temperature 356 - 446 °FInjection
Zone 1 360 - 450 °FExtrusion
Zone 2 370 - 460 °FExtrusion
Zone 3 380 - 470 °FExtrusion
Zone 5 390 - 480 °FExtrusion
Die Temperature 390 - 480 °FExtrusion
Mold Temperature 95.0 - 120 °FInjection
Injection Pressure 200 - 800 psiInjection
Back Pressure 25.0 - 100 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0924 / 237415

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.