MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Capron® 5202 HS BK-102 Nylon 66 (Dry)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: Capron 5202 HS BK-102 is an unfilled, heat stabilized, pigmented black nylon 6,6, injection molding compound. It combines strength and stiffness as well as excellent chemical resistance. The addition of heat stabilizer system extends its retention of properties at elevated temperatures.

Capron 5202 HS Bk-102 is generally recommended for applications requiring slightly higher temperature and stiffness, such as engine component, power tools guides, straps and other hardware.

Data provided by Allied Signal.

Processing: Max. water content 0.25%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 280-305 degC (536-581 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF) is recommended, but temperatures of as low as 45 degC (113 degF) and as high as 105 degC (221 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO data
Moisture Absorption at Equilibrium 2.5 %50% RH; 23°C; ISO data
Water Absorption at Saturation 8.5 %in water; 23°C; ISO data
Viscosity Measurement 55Formic Acid Viscosity; ISO data
Linear Mold Shrinkage 0.015 cm/cmASTM Data MD
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 85.0 MPaASTM value at 50 mm/min.
 86.0 MPaISO value at 50 mm/min.
Elongation at Break 15 %Nominal
 15 %Nominal
Elongation at Yield 3.0 %ASTM Value at 50 mm/min.
 5.0 %ISO Value at 50 mm/min.
Flexural Yield Strength 135 MPaASTM Data
Flexural Modulus 3.24 GPaASTM Data
Poissons Ratio 0.35ISO data
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CASTM and ISO test
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CASTM Data
Flammability, UL94 V-2
@Thickness 0.700 mm
 V-2
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Drying Temperature 85.0 °CSee Materials Notes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei Leona® 1300S Nylon 66
Akro-Plastic Akromid® A3 1 black (2417) PA 66 Conditioned
BASF Capron® 5202 HS Blend Nylon 66 (Dry)
Kuraray Genestar™ G1300A-M41 Nylon, 30% Glass Filled
Mitsubishi Chemical Advanced Materials Nylatron™ 101 / Ertalon™ 66 SA PA66 Extruded, Unfilled, Type 66 Natural and Black

PALC05 / 23799

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.