MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Schott IOG-10 Phosphate Laser Glass
Categories: Ceramic; Glass; Optical

Material Notes: IOG-10 is an alkali-zinc-silicate glass developed for use in passive waveguide devices, which are fabricated by ion exchange in a molten KNO3 or AgNO3 salt bath. IOG-10 glass can be codoped with erbium and ytterbium for use in active devices. However, the laser properties of Er/Yb doped IOG-10 are inferior to those realized in a phosphate glass host, such as IOG-1 or IOG-2. IOG-10 devices are discussed in “Ion exchanged waveguide lasers in Er/Yb codoped silicate glass,” Appl. Optics, 38 [33] 6879-6886 (1999).

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.71 g/cc
 
Chemical PropertiesOriginal ValueComments
Acid Class, SR 1.0pH = 0.3 at 25 °C
Alkali Class, AR 1.0pH = 12 at 50 °C
Stain Resistance Class, FR 0.00pH = 4.6 100 h at 25 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 5200.1/20
Modulus of Elasticity 71.0 GPa
Poissons Ratio 0.24
Fracture Toughness 0.710 MPa-m½KIC
Shear Modulus 28.6 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 68.0 µm/m-°C
@Temperature 20.0 - 40.0 °C
 93.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.770 J/g-°C
Thermal Conductivity 0.920 W/m-K
Transformation Temperature, Tg 569 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.53
 1.518
@Wavelength 1540 nm
 1.521
@Wavelength 1000 nm
Transmission, Visible 56.6 %
 
Descriptive Properties
Climatic resistance1Water Vapor at 40 – 50 °C for 30 h
Thermal Diffusivity4.4 [10-7 m2/sec]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
Tricalcium-Phosphate (TCP), CA3(PO4)2
Thermal Ceramics Kaolite 2200-HS Gunning Insulation Castables
Tetracalcium-Phosphate, Ca4PO9
Phosphate Rock

CSGT9936 / 183189

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.